To make asem
Carefully purify lead with pitch and bitumen, or tin as well; mix cadmia and litharge in equal parts with the lead. Stir till the mixture becomes solid. It can be used like natural asem.
[Reduction in the furnace must here also be assumed. The soft white alloy so obtained must have been a cheap and poor substitute for electrum or silver.]